Project Info

77 Forest Lane Drive

2015
Areas Repaired Ledge Beams, Expansion Joints, Wall / Ceiling Patching and Waterproofing, Crack Injection
Repair Types Polyforce Plus Patching with Basalt and Concrete, Fiberglass Coating, Polyforce Plus Crack Injection, PolyFlex Ledge Beam and Expansion Joint Injection
Issues Active leaks, Membrane Failure, Concrete Delamination, Concrete Cracks

Technical Details

Facts

In accordance with third-party testing, the repaired surfaces are rated to the following:

Polyforce Plus

  • 25 years of useful life
  • 0% water permeation
  • Polyforce Plus is rated to expand and contract with concrete
  • The entire surface and volume of the slab is "monolithic"
  • Compressive strength of 85 MPa
  • Polyforce Plus mixed with Basalt reaches a compressive strength of 150 MPa
  • Adhesive strength of 1.85 MPa (original concrete has only 1.2 MPa of a tensile strength, so the bond is stronger than the concrete itself)
  • Repair is 60% cost of a traditional repair

Facts

In accordance with third-party testing, the repaired surfaces are rated to the following:

PolyFlex

  • Application of PolyFlex from the negative side reduces cost by 90% when compared to the traditional method of repair
  • 10 years of useful life
  • 0% water permeation
  • PolyFlex is able to expand and compress 200%
  • 200% expansion and compression does not affect adhesion or tensile strength of PolyFlex

Customer Service
Workmenship / Quality
Repair Capital Cost Saving
Issue Remediation